Wednesday, August 18, 2010

Re: [MW:6547] FLUX

Hi,

yesterday i sent you about SAW fluxes for Inconel.


For normal fluxes please find below the details.


If fluxes comes with drums no need to baking before opening.

But if fluxes comes with bags,it shall be bake  to 300 - 350 degrees with 2hours to 10 hours.


Thanks & Regards,


(karthik)


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 8/17/10, Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com> wrote:

From: Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com>
Subject: [MW:6540] FLUX
To: materials-welding@googlegroups.com
Date: Tuesday, August 17, 2010, 3:29 PM

WHAT IS THE TEMPERATURE OF  HEATING OF FLUX IN SAW?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...