Re: [MW:6570] EA 981/15 electrdes

http://www.elmics.ru/material/el/el0302_e.htm# (check the attachment)

On Wed, Aug 18, 2010 at 7:26 PM, mayur purwant <mayur15787@yahoo.co.in> wrote:
What Parameters (Current, Travel spee) should I used for EA981/15 electrodes.
 
 
Regards,
Mayur Purwant
Welding
Godrej & Boyce


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...