Hi,

TU37 is a Carbon steel Seamless Boiler tube..Find below the equivalents.

TU37C equivalent to ST35.8  and P235GH/EN10216-2.

TU37B equivalent to ST37  and P235TR1/EN10216-1 and BS3601-S360


Thanks & Regards,


(karthik)


Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 8/19/10, Vertex Engineers <vertexnaik@rediffmail.com> wrote:

From: Vertex Engineers <vertexnaik@rediffmail.com>
Subject: [MW:6588] Material:TU 37 b mean which grade?
To: materials-welding@googlegroups.com
Date: Thursday, August 19, 2010, 5:18 PM

Can Any body tell TU 37 b meanwhich grade is this?

THis is used for piping including, fitting like reducer, elbow, etc.

Thanks

Devang Naik


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...