COLD DRAWN SEAMLESS TUBE, IN MILD STEEL, HUE TU 37 B, ACCORDING TO STANDARD NF-EN10305-4 AND ST 37-4 AND TO STANDARD DIN 2391 C. BRIGHT ANNEALING TUBE IN NEUTRAL ATMOSPHERE (NBK). PL. REFER ATTACHMENT
________________________________________
From: materials-welding@googlegroups.com [materials-welding@googlegroups.com] On Behalf Of DINESH TIWARI [dinesh29tiwari@yahoo.com]
Sent: Thursday, August 19, 2010 4:40 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6590] Material:TU 37 b mean which grade?

Devang ,

Go to the below link you will find it useful .

http://www.globalmega.com/products/materialtable.htm


Best Regards
------------------
Dinesh Tiwari


________________________________
From: Vertex Engineers <vertexnaik@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, 19 August, 2010 2:18:18 PM
Subject: [MW:6588] Material:TU 37 b mean which grade?

Can Any body tell TU 37 b meanwhich grade is this?

THis is used for piping including, fitting like reducer, elbow, etc.

Thanks

Devang Naik


Filtered by Hosted Filtering

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...