Hi

In ASME Sec IX, QW 403.6 and QW 403.8 are welding variables to be referred for PQR.

For Welder Performance qualification thickness of weld metal qualified, please refer QW-452.1(b).

Regards

Prem Nautiyal


On Thu, 19 Aug 2010 22:33:41 +0530 wrote
>Dear All



BY ASME Sec IX for Welder Thickness range qualification, I am

referring QW 403.8 thats tells tat refer QW 451.1.

but wats QW 403.6 says? If we refer QW 451.1 is correct or not?



If we see welding variables QW 403.8 is essential variable & QW 403.6

is supplementry variables. wat SEC IX says



For welder thickness range qualification wat we have to refer? either

403.8 or403.6 ?

Pl explain this?



Regards

Srinivas



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...