Dear Members,
Appreciate if you could provide me some information on the issue, During a PQR, manufacturer has used electrode F6A0-EM12 to weld plates A516 Gr. 65, welding procedure is SAW. Below is the comparison, between the tensile strength of the electrode,
comparison table
WELDING FLUX F6A0 PLATE flux certificate(see attachment) Strength of the plate material
REFER TO SFA 5.17 ASTM A516, GR65 test result Test Result
Tensile Tensile tensile tensile
60,000~80,000 psi 65000~85,000 psi 72289 psi (500MPa) 68875 psi (475 Mpa)
Our client says that the selected electrode is not suitable for Gr. 65c plates. Is it correct?They say that the electrode shall be selected considering the minimum strength ( for this electrode minimum strength is 60, 000 PSI), and therefore it is not suitable for a plate with minimum strength value equal to 65000 PSI .
As you can see in the above table tensile test value for the electrode is 72289 PSI, but still the client is not ready to accept the use of this electrode.
Please advise.
Regardsa
MS
_
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment