----- Original Message -----From: A DSent: Friday, August 20, 2010 8:47 PMSubject: Re: [MW:6612] MW:6593- Re: value of ferrite contentHiThanks for your valuable message.But my client specification give acceptance range for duplex weld acceptance is 3 to 10 FN only.Louis
From: GOSWAMI Pradip -THERMAL <pradip.goswami@opg.com>
To: materials-welding@googlegroups.com
Cc: alouis1972@yahoo.co.in
Sent: Fri, 20 August, 2010 2:30:43 AM
Subject: [MW:6602] MW:6593- Re: value of ferrite content
Hi Louis,
Please find the following documents for your reference. The first one (extracted from Metals Handbook) is the WRC-1992 diagram for predicting ferrite in stainless steel weld metal. For duplex stainless steel the concept is based on extended ferrite no, shown in the diagram.
The second paper from Avesta, shows the formula for conversion of % Ferrite to FN.
· Volume Percent Ferrite = 0.55 EFN + 10.6
This formula looks to be accurate as Ferrite 65% by volume fraction turns out to 100 FN approx.
You may use this formula to convert form Volume % ferrite to FN, as asked below.
Thanks.
Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Ontario Power Generation Inc.
Email-pgoswami@sympatico.ca,
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of A D
Sent: Thursday, August 19, 2010 9:48 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6593] Re: value of ferrite content
Dear all,
Can anybody give reference details what is ferrite no range will get if duplex weld ferrite content is 30-60%.
Louis
QC Engineer
Singapore
From: Yoon <ych93@hotmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Tue, 17 August, 2010 1:23:33 PM
Subject: [MW:6536] Re: value of ferrite content
above value mentioned by Mr Bathula is for weld metal, not base material.
Regards
On Aug 17, 2:02 pm, "Bathula Raghuram (Mumbai - PIPING)"
<R.Bath...@ticb.com> wrote:
> For Duplex SS it would be 30-60% and austenitic SS 3-10% (except 310)
>
>
>
> -----Original Message-----
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Yoon
> Sent: Tuesday, August 17, 2010 10:16 AM
> To: Materials & Welding
> Subject: [MW:6533] Re: value of ferrite content
>
> The chemical analysis of S31803 is designed to obtain 50% ferrite contents.
> The range of ferrite content depends on actual chemical contents.
>
> I think carbon content for C.S or S.S is not important. Anyway ferritic carbon steel : approxi. 100%, austenitic stainless steel:
> approxi. 0%.
>
> Regards,
>
> On Aug 17, 10:38 am, skrie85 <skri...@yahoo.com> wrote:
> > What the range value/percentage for ferrite content of duplex (SA240
> > UNS 31803) , Stainless steel and Carbon steel?
>
> Filtered by Hosted Filtering- Hide quoted text -
>
> - Show quoted text -
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Monday, August 23, 2010
Re: [MW:6632] MW:6593- Re: value of ferrite content
Hi Louis,
FN level given by you is seems to be very low.
Might be this one for the ASS.
Regards,
K.Babu
Subscribe to:
Post Comments (Atom)
[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point
Dear Experts. If anyone having presentation of WPS,PQR and WPQ as per ASME SEC.IX in power point then please share . Regards Sanja...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment