Re: [MW:6638] Paint Consumption

1.Study the technical leaflet of paint which needs to be applied.
2.Check ,what is the TSR(theoretical spreading rate) sq.m per litre
3.Consider PSR(practical spreading rate) as 0.5XTSR. sq.m per litre
4.Caculate your job area which you want to paint in sq.m.
5.Divide this area by sq.m at (3) to arrive at total paint qty in litres.
Regards
Aarpee

On Mon, Aug 23, 2010 at 10:45 AM, Ramesh Barot <rameshnbarot@yahoo.com> wrote:
Dear All,
 
Can anybody guide me how can we calculate the paint consumption on steel?
 
Thanks in Advance,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...