RE: [MW:6639] PWHT Requirement

Please specify you base material specification, thickness, type of weld, service restriction if any and code of construction.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ankur Mande
Sent: Monday, August 23, 2010 11:07 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6637] PWHT Requirement

You have to simulate the weld in the PQR exactly similar to that being actually done on the job. If your weld shall be going under PWHT in you job, then yes you have to perform pwht on the pqr also. If not then pqr shall not call for pwht.
 
Ankur.

On Mon, Aug 23, 2010 at 9:46 AM, subrata das <sdas@pkgroup.org> wrote:

Dear All

I have a job in which Alloy Steel to Non-ferrous pipe to be weld. While conducting PQR Is it necessary to do PWHT on the test coupon.   

Regards

Subrata Das


No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...