base material specification : UNS N10276 PIPE TO A182 GR. F91 FLANGE
thickness : 6.35 MM
type of weld : SINGLE ‘V’ GROOVE
service : BOILER FEED WATER SHALL BE INJECTED THROUGH IT.
Regards
Subrata Das
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Monday, August 23, 2010 11:21 AM
To: 'materials-welding@googlegroups.com'
Subject: RE: [MW:6639] PWHT Requirement
Please specify you base material specification, thickness, type of weld, service restriction if any and code of construction.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ankur Mande
Sent: Monday, August 23, 2010 11:07 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6637] PWHT Requirement
You have to simulate the weld in the PQR exactly similar to that being actually done on the job. If your weld shall be going under PWHT in you job, then yes you have to perform pwht on the pqr also. If not then pqr shall not call for pwht.
Ankur.
On Mon, Aug 23, 2010 at 9:46 AM, subrata das <sdas@pkgroup.org> wrote:
Dear All
I have a job in which Alloy Steel to Non-ferrous pipe to be weld. While conducting PQR Is it necessary to do PWHT on the test coupon.
Regards
Subrata Das
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.