William ,
 
80 degree is allowable tilt in the production weld not for the qualification purpose.
 
Regards,
 
K.Babu
Singapore
 
----- Original Message -----
Sent: Monday, August 23, 2010 3:24 PM
Subject: [MW:6643] weld test positions

Guys,

In accordance with ASME IX QW461 positions.

If I test welders on plate and tilt the joint to 80 degrees does that mean on one test butt weld I can qualify my welders for 3G and 4G?

Comments please.

 

Lusk

Senior Welding Engineer

Tel. : +966(4)3961171

Ext. : 344

Mobile+966 55 880 0431

E-mail : william.lusk@yanbusteel.com

billlusk66@yahoo.com

 



This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...