Re: [MW:6660] ELECTRDOE STRENGHT REQUIRMNET FOR PLATE GR65

Sujeeth,
              In all PQR testing as per ASME SEC-IX requires Tensile strength only .How can you calculate based on Yield strength.
 
vaithiyanathan

 
On 8/22/10, Sujeet Sangle <sujeet.sangle@swiber.com> wrote:

We should select the consumable with the YS and no TS properties .

 

Regards,

 

Sujeet

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of B.Vaithiyanathan
Sent: Sunday, August 22, 2010 5:56 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6625] ELECTRDOE STRENGHT REQUIRMNET FOR PLATE GR65

 

Always the welding electrode should meet Base material strength .By this way the electorde slection should be F7A0 .

 

Regards,

Vaithiyanathan,

 



 

On 8/22/10, Syed Moin <Syed.Moin@gerabgroup.com> wrote:

Dear Members,

Appreciate if you could provide me some information on the issue, During a PQR, manufacturer has used electrode F6A0-EM12 to weld plates A516 Gr. 65, welding procedure is SAW. Below is the comparison, between the tensile strength of the electrode,

comparison table                               
        WELDING FLUX F6A0       PLATE   flux certificate(see attachment)        Strength of the plate material 
        REFER TO SFA 5.17       ASTM A516, GR65 test result     Test Result    
        Tensile Tensile tensile         tensile
        60,000~80,000 psi       65000~85,000 psi         72289 psi (500MPa)     68875 psi (475 Mpa)    
                                       
Our client says that the selected electrode is not suitable for Gr. 65c plates. Is it correct?

They say that the electrode shall be selected considering the minimum strength ( for this electrode minimum strength is 60, 000 PSI), and therefore it is not suitable for a plate with minimum strength value equal to 65000 PSI .

As you can see in the above  table tensile test value for the electrode is 72289 PSI, but still the client is not ready to accept the use of this electrode.

Please advise.

Regardsa

MS

 


______________________________________________________
CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Disclaimer: If you are not the intended recipient, you must not copy, distribute or use it for any purpose, nor disclose its contents to any other person. Any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the company. The company will not accept any liability in respect of such communication, and the employee responsible will be personally liable for any damages or liability arising from, but not limited to, defamatory statements, infringement of copyright or any other legal right. Please delete the email and notify the sender immediately if you receive this in error.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...