Re: [MW:6700] How to protect Serration of Flanges during Hot dip galvanization

Aly :

I have done it before,and it just working fine. It is true that there are small amount of melting zinc will fill the gaps between serration but per my past experience there are still enough roughness to hold the gasket.

I did it on 2 ", 4 " and 6 " flanges for your info.

Regards
Richard Bonardo
QA/QC Engineer
PHE-ONWJ



From: Aly <mhaskar.aly@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, 24 August, 2010 1:03:42 AM
Subject: Re: [MW:0] How to protect Serration of Flanges during Hot dip galvanization

The Galvanization temperature is 450 Deg C . 
 
 
 
-------Original Message-------
 
Date: 23/08/2010 14:04:22
Subject: Re: [MW:6656] How to protect Serration of Flanges during Hot dip galvanization
 
AT WHAT TEMPERATURE HOT DIP GALVANIZATION IS DONE?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
FREE Animations for your email - by IncrediMail! Click Here!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...