Hi,
 
Control the maximum range to control heat input.

Thanks & Regards
Muhammed Ibrahim PK



On 25 August 2010 17:34, ayys4u <ayys4u@gmail.com> wrote:
Dear All,

Can any one help me!

PQR Qualified with an amperage of min 350 and max 550.
As per AWS D1.1, Allowable Variation in Amperage for WPS  is 10 %.
How should i consider this 10%.

Case 1
Should i Consider lesser 10 % lesser to  PQR's Min Amperage and
Greater side 10 % to the max PQR Amperage.

Case 2
 Or Should i consider 10% min max of Average of PQR Value.

Which case is correct?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...