Re: [MW:6711] Reg Range of Amperage in WPS

CASE 1 is applicable for SAW/GMAW/FCAW
For SMAW : To a value not recommended by manufacturer

 
G.S.Arora
B4-103 LaHabitat
Opp Marutinandan Villa
Near Aayna Shopping Complex
Off SG Road Thaltej
AHMEDABAD-380054
Ph: 91-9725262404


--- On Wed, 25/8/10, ayys4u <ayys4u@gmail.com> wrote:

From: ayys4u <ayys4u@gmail.com>
Subject: [MW:6707] Reg Range of Amperage in WPS
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, 25 August, 2010, 7:04 PM

Dear All,

Can any one help me!

PQR Qualified with an amperage of min 350 and max 550.
As per AWS D1.1, Allowable Variation in Amperage for WPS  is 10 %.
How should i consider this 10%.

Case 1
Should i Consider lesser 10 % lesser to  PQR's Min Amperage and
Greater side 10 % to the max PQR Amperage.

Case 2
Or Should i consider 10% min max of Average of PQR Value.

Which case is correct?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...