RE: [MW:6722] Charpy impact Test qulaification for an existing PQR

what is your material, job thickness range and code of construction?


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: Thursday, August 26, 2010 5:31 AM
To: materials-welding@googlegroups.com
Subject: [MW:6716] Charpy Test

Hi There,

 

We have an existing WPS, The existing WPS doesn’t have a cold service specification, and we would like to do a test coupon from that WPS and have it charpy tested, so we can revised the existing WPS. Now the requirement of the client is -70 degrees Celsius. Is that alright or do we have to do another PQR? Code is ASME IX.

 

 

Thank you,

 

Larry Zarate


No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...