Base metal impact test is mandatory for API5LX52PSL2 at 0 deg C with values,27J average and 22 J minimum.Welding procedure does not call for impact test if MDMT is warmer than -29 deg C.
Regards
Aarpee


 
On Thu, Aug 26, 2010 at 1:09 AM, Sajish <sajishjm@gmail.com> wrote:
Hi,

Can anyone clarify wether impact testing is required for API 5L PSL2
Code of construction is ASME B31.8
and for B31.4
Would be qualifying the procedure as per ASME Sec IX.

Thanks in advance
Sajish

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...