Re: [MW:6748] Re: Pressure vessel in Austenitic-Ferritic Stainless Steel

Dear Mr. Herman Pieper
2010 edition will be applicable from Jan 2011, current applicable edition will be 2007+addenda 2009. however your designer/client should specify based on which edition/addenda this vessel should be designed.

On Fri, Aug 27, 2010 at 5:39 PM, hpi001 <pieper-qsi@kpnmail.nl> wrote:
Dear Mr. Raghuram,

Grade was not known by me right know, I needed to find a alternative
for 1.4462. But with the specification mentioned by you I find out
that UNS 32205 is the alloy we need to specify in our purchase order.
I only have a copy available of the 2007 edition of ASME, what is your
opinion can I still use this or do I really have find a copy of the
2010 version?

Best Regards,

Herman Pieper

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...