Re: [MW:6771] Any WPS for P91 Material without PWHT

All asme bpvc sections require pwht for p91


  From: "Mohamed Farook" [asfaruk@gmail.com]
  Sent: 30/08/2010 12:00 ZE8
  To: <materials-welding@googlegroups.com>
  Subject: [MW:6769] Any WPS for P91 Material without PWHT


Dear friends,

 

Greetings to all,

 

Please advise me if you have WPS for P91 material without PWHT….

 

PWHT is time consuming..

 

Thanks and Regards,

asfaruk