Monday, August 30, 2010

Re: [MW:6779] Polarity qualification?

Hi,
For Welder Qualification,SMAW polarity is not an essential variable(QW353).If he qualifies with DCEP he can qualify for both.
But for PQR,Change in polarity is a supplementary essential variable.Then you have to follow QW409.4.
 
 
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sat, 8/28/10, prem_nautiyal <prem_nautiyal@rediffmail.com> wrote:

From: prem_nautiyal <prem_nautiyal@rediffmail.com>
Subject: Re: [MW:6777] Polarity qualification?
To: materials-welding@googlegroups.com
Date: Saturday, August 28, 2010, 6:20 PM


Hi

If you are referring ASME Sec IX, then as per the table of QW-253 which talks about welding variables procedure specifications, refer QW-409.4 (Electrical characteristics), change in current or polarity is considered as supplementary essential variable for Impact requirements and Non-essential if you don't have any Impact requirements.


Regards

Prem Nautiyal

On Sat, 28 Aug 2010 15:26:12 +0530 wrote
>Dear all





If one qualifies in DCEP for SMAW,

Whats the range qualified for those either DCEP only or both (DCEP&

DCEN)?

any limits given in specs? where?





Thanks



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...