Tuesday, August 31, 2010

RE: [MW:6796] Propane or butane to preheat

Nothing wrong in it, gas used for heating is not a variable to consider.

sent from my handheld
-----Original Message-----
From: eduardocalva@hotmail.com
Sent: 31/08/2010 12:00:40 am
Subject: [MW:6794] Propane or butane to preheat

Could all of you tell me the difference between preheat with propane
and butane?, If a WPS is qualified by preheating with propane but
butane is used in production welds is wrong?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...