Hi Shashank,
 
Thanks for attachment.
I found on it the T23 filler metal for 2.25Cr-1Mo. I will make a comparison between it and others that Pgoswami has suggested.
 
Thanks for your interest Shashank.
 
L. Carlos Flores
Piping Team Leader
Oficina:(993) 310 8100 Ext. 106
Celular:(993) 250 6610



 



Date: Tue, 31 Aug 2010 05:24:01 +0530
From: nach_sam@yahoo.com
Subject: Re: [MW:6791] A 217 Gr WC9
To: materials-welding@googlegroups.com

Hi Luis,
I hope the attached Bohler data sheet will be useful. Please let me know if you found in it what you looked for.
Thanks,
Shashank Vagal

--- On Mon, 30/8/10, Luis Carlos <carlosflores126@hotmail.com> wrote:

From: Luis Carlos <carlosflores126@hotmail.com>
Subject: [MW:6788] A 217 Gr WC9
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Monday, 30 August, 2010, 10:06 PM

Hello,

Could someone tell me please what is the best filler metal to make a
buttering over A-217 Gr WC9 base metal.

Are there special recommendations?

I will appreciate answers!

Luis Carlos

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...