Bill
See QW-120, QW-121 and QW-131.
Regards
John du Plessis
Technology Manager
Tel: +27 (11) 298 2100
Tel: +27 (11) 298 2103 (Direct)
Fax: +27 (11) 836 6014
This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of William Lusk
Sent: 23 August 2010 09:40 AM
To: materials-welding@googlegroups.com
Subject: RE: **** SPAM **** [MW:6645] RE: 6643] weld test positions
John,
Thanks for your reply can you please explain why not.
Regards
Bill
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of John Du Plessis
Sent: Monday, August 23, 2010 10:36 AM
To: materials-welding@googlegroups.com
Subject: **** SPAM **** [MW:6644] RE: 6643] weld test positions
No
John du Plessis
Technology Manager
Tel: +27 (11) 298 2100
Tel: +27 (11) 298 2103 (Direct)
Fax: +27 (11) 836 6014
This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of William Lusk
Sent: 23 August 2010 09:24 AM
To: materials-welding@googlegroups.com
Subject: [MW:6643] weld test positions
Guys,
In accordance with ASME IX QW461 positions.
If I test welders on plate and tilt the joint to 80 degrees does that mean on one test butt weld I can qualify my welders for 3G and 4G?
Comments please.
William Lusk
Senior Welding Engineer
Tel. : +966(4)3961171
Ext. : 344
Mobile+966 55 880 0431
E-mail : william.lusk@yanbusteel.com
billlusk66@yahoo.com
This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.
This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.
No comments:
Post a Comment