Dont confuse with the allowance given in QW461.The 80degrees is a allowable angle tolerance while the welder doing production weld after qualification.But while doing qualification it should be in the angle as specified in QW461.If you qualified the production weld for the wlder qualification pls.make sure the welder weld in the position according to QW461.If you qualify the production weld in 4G position, You cannot qualify for vertical position(3G).You can give them only for F,O(Flat and overhead).
 
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Mon, 8/23/10, William Lusk <William.Lusk@yanbusteel.com> wrote:

From: William Lusk <William.Lusk@yanbusteel.com>
Subject: RE: **** SPAM **** Re: [MW:6650] weld test positions
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Monday, August 23, 2010, 3:27 PM

 Mr Babu,

So if I qualify the welders on production weld I can then give them 3G & 4G qualifications is that what you are saying?.

Regards

Bill

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Monday, August 23, 2010 11:11 AM
To: materials-welding@googlegroups.com
Subject: **** SPAM **** Re: [MW:6648] weld test positions

 

William ,

 

80 degree is allowable tilt in the production weld not for the qualification purpose.

 

Regards,

 

K.Babu

Singapore

 

----- Original Message -----

From: William Lusk

Sent: Monday, August 23, 2010 3:24 PM

Subject: [MW:6643] weld test positions

 

Guys,

In accordance with ASME IX QW461 positions.

If I test welders on plate and tilt the joint to 80 degrees does that mean on one test butt weld I can qualify my welders for 3G and 4G?

Comments please.

 

Lusk

Senior Welding Engineer

Tel. : +966(4)3961171

Ext. : 344

Mobile+966 55 880 0431

E-mail : william.lusk@yanbusteel.com

billlusk66@yahoo.com

 

 


This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.


This e-mail and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the system manager. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. Finally, the recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this e-mail.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...