Sunday, January 2, 2011

[MW:9048] Repair of Body cracks for A 217 Gr WC6

Dear All,

We have noticed multiple crack during the replica check in the control valve body ( Material A 217 Gr WC6 , size 2 " X 2500 RTJ, H2 service) during the fire incident at our Hydrocracker plant. We would like to carry out the repair jobs for the same,

Kindly share your experience and also advise whether advisable or not. Also share the WPS and cautions to be followed if repair performed by anyone in the group.

Vinod

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...