[MW:9088] Welder qualification Position range doubt? 4G doubt qualifies for?

Dear All

If one welder qualifies in 4G...
As of practical he qualifies to all structural position tat 3g, 2G.

as per AWS D1.1, he only qualifies for 4G only - overhead.

pl clear me.. That if welder qualify to weld all position? or is he
only qualify for overhead?

Thanks
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...