[MW:9098] WPS and PQR for P 1 material and P 5

Dear All !
Could you help me any one... We have IS 2062 material
for rail welding... the manufacturer recommend for E 7018 for root,
hot and filling and E9018 for capping on IS 2062... My Question is how
to allow E 9018 on IS 2062? Both electrodes have different A No...
That is essential variable... So please give advice...

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...