Dear All, Further to my below quirey,i will add up some more points which relate to that. Material: SA213 TP304H- Tube-Dia-101.6x8.55mm.thk. Design Code-API530 Construction code : Sec.VIII,Div.1/B31.3 Inside bending radius - 1750mm OD - 3500mm Design temp - 300 degree celsius According to UHA44 or B31.3,need postfabrication heattreatment or not? Thanks & Regards, (Karthik) Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282 --- On Tue, 1/11/11, Karthik <karthik6684@yahoo.com> wrote:
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment