The above material has sollution annealed at 1040 degree celsius from material manufacturer.We are going to make coiling of these tubes(Coil Dia-3.5Mx8M(height) ).
Quirey:
01. Does sollution annealing to be done again after coiling of these tubes? because our customer asked us to do Sollution annealing after coiling.(they referred to ASME Sec.II-Part-A)Also our customer not aware of API530 requirements.Also I dont have API530 book.
 
02.Please give, is there is any requirement as per API530?

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...