Tuesday, January 11, 2011

[MW:9183] Effect of active titanium ions on carbon steel in presence of moisture

Dear experts

A 3" catalyst drain of CS has failed locally at many locations,minimum
thickness of 1.3mm against 5.5mm is observed after 1.5 months of
operation.


Service; TiCl4+MgCl2 with traces of hexane having moisture of unknown
value
Temp; 80degC max.

Press; 0.5kg

Any experiences with Ti+ ions effects on carbon steel and suitable
metallurgy under present condition is highly appreciated.

regards
yogeshkumar

inspection engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...