Dear All,


1. What will happen when Mo content of SA 516 Gr. 70 become ZERO?? As
per SA 20 only maximum level restriction is mentioned when that
specific material content become zero is it acceptable as per Code??

2. What is the difference between Normalized Rolled and Normalized and
supply condition as "as rolled"?

3. If Nb content of SA 516 Gr.70 is higher than what is mentioned in
SA 20 Table 1. and our customer is ready to accept it as per Table 1
Note D, Do we need to mention it in Technical Delivery Condition?

4. For Super Duplex, what exactly meant by Finish Nr. 1?? If our
requirement is White pickled steel, can I accept it just with the word
Finish Nr. 1??

5. Is there any specific Normalizing temperature and the duration to
be followed for SA 516 Gr. 70 in Code??

Regards

Akhil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...