Friday, January 14, 2011

[MW:9217] Welding of P9 & P91 material

This is not a dissimilar weld, however consider it as special/critical weld in terms of Weldability, thermal treatment ...

You can use either E80XX-B8 or E 90XX-B9, however separate PQR is required.

 

From: piping_valves@yahoogroups.com [mailto:piping_valves@yahoogroups.com] On Behalf Of desaid@toyoindia.com
Sent: Friday, January 14, 2011 1:05 PM
To: materials-welding@googlegroups.com
Cc: piping_valves@yahoogroups.com
Subject: [piping_valves] <Security Level 2>Welding of P9 & P91 material

Dear Respected members,

Which electrodes are used for welding of P9 & P91 material, Is this considered as dissimilar welding & Special Welding.
Can the electrode & process used for welding P9-P9 material be used for welding P9-P91 material also.

Your reply shall be highly appreciated.

Thanks & Regards,
Dhwani Desai
Planning & Piping Dept.
Ext.-7681


No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...