[MW:9225] Re: P43 and P45

no, you can't, need separate qualification

On Jan 15, 12:32 pm, VENKATA SWAMI REDDY KARRI <kvsreddy...@gmail.com>
wrote:
> we have a wps and pqr for p 43 material of inconel, filler wire
> incrmo3.But  we can use it for
> p45 material uns no n08926? this material grop alloy-622 and filler
> wire nicrmo-3 both filler wire is same but gtaw process P number is
> assencial as per asme sec 9. i have doubt to use it are not

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...