[MW:9226] BRANCH 3/4" FROM 4" LINE LP STEAM

Dear All,

Is it possible to weld pipe 3/4" to pipe 4" in LP steam service  in the form of Pipe to Pipe (we have no any sockolet or Halfcoupling, ...)?

Does it need REINFOCEMENT?

your reply is highly appreciable.
 
Regards
Zarei

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding