[MW:9229] RE: 9227] P11 SR holding time

Dear Vasu:

As far as I know in All STD Holding time has been specified as minimum and you can increase holding time ,I think holding time  will have negative effect just on Toughness properties, you know holding time also is supplementary essential in ASME IX.

 

Regards

Bazrafshan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of srinivas rao
Sent: Saturday, January 15, 2011 6:42 PM
To: materials-welding@googlegroups.com
Subject: [MW:9227] P11 SR holding time

 

Dear All,


Pls let me know , In Stress relieving of P11 joints will there be any effects in properties if we maintain the Holding time more than the specified?

Regards

Vasu
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.