Tuesday, January 18, 2011

[MW:9282] RE: 9280] what is ASTM G 48 test method in DSS & SDSS

It is standard test method for pitting and crevice corrosion resistance of stainless steel and related alloys by use of ferric chloride solution.

 

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: Tuesday, January 18, 2011 9:49 AM
To: materialswelding
Subject: [MW:9280] what is ASTM G 48 test method in DSS & SDSS

 

Dear all,
                 pls explain in detail what is ASTM G48 and why and where it is used in welding of DSS & SDSS.

Is it required for only WPS & PQR or also for welder qualification also?

thanks,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...