Wednesday, January 19, 2011

[MW:9322] QW-407.2

Dear Friends,
 
i need correct interperation of the Clause of mentioned below.
 
thanks and regards
 
 
 
QW-407.2
A change in the postweld heat treatment

(see QW-407.1) temperature and time range

The procedure qualification test shall be subjected to

PWHT essentially equivalent to that encountered in the

fabrication of production welds, including at least 80% of

the aggregate times at temperature(s). The PWHT total

time(s) at temperature(s) may be applied in one heating

cycle

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...