Dear All,
Design code ASME sec viii, div 1,
Pig trap barrel material P460 ML1 (TMCP treated) , Thickness 40mm
welded to
A765 End closure, Thickness 60mm,
Since CE value of P460 ML1 is 0.46% and design code mandate PWHT with nominal thickness (40mm),
Can somebody give me an insight of PWHT effect on P460 ML1 mechanical properties and appropriate PWHT temperature?
Regards
Manpreet Singh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point
Dear Experts. If anyone having presentation of WPS,PQR and WPQ as per ASME SEC.IX in power point then please share . Regards Sanja...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment