Dear Sir:
Please see attached table.
I hope it would be useful.
Regards
Bazrafshan
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of praveen nair
Sent: Wednesday, January 19, 2011 2:33 PM
To: materials-welding@googlegroups.com
Subject: [MW:9330] selction of filler rods for similar and dissimilar metals
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.