One more doubt..
If joint configuration like Joint Between 80 degree to 100 degree. we
have to consider leg size for Table 5.8.
& Joints less than 80 degree & greater than 100 degree we have to
consider Throat size as weld size for Table 5.8.
am i correct or not?
pl advise me.
Thanks
Srinivas
On Jan 19, 11:37 pm, Karthik <karthik6...@yahoo.com> wrote:
> Hi,
> As per AWS-Section5-Fig.5.4 weld size means - Lug size.
>
> Thanks & Regards,
>
> (Karthik)
>
> Karthikeyan.S
> QA/QC Manager
> Getabec Energy Co.,Ltd.
> 379,Moo6,Soi8,Nikhomphatana,
> Rayong-21180,
> Thailand.
> Phone: 0066 38 897035-8 (Off)
> Fax: 0066 38 897034
> Hand Phone: 0066 892512282
>
> --- On Wed, 1/19/11, Srinivas Engr <srinivas.gmsr...@gmail.com> wrote:
>
> From: Srinivas Engr <srinivas.gmsr...@gmail.com>
> Subject: [MW:9333] AWS Table 5.8 doubt???
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Wednesday, January 19, 2011, 10:50 PM
>
> Dear all,
>
> AS per AWS.I knw tat for fillet weld sizes we have to refer Table 5.8.
> My doubt is they given as weld size.
> weld size refer to throat or leg length? which one tat refers?
> clear me
>
> Thanks & Regards
> Srinivas
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment