[MW:9375] RE: Minimum thickness Qualification

What is the MOC? If the PQR is qualified on 20mm with impact, and there is no PWHT above Ac3 temp

Then WPS qualification range will be 16-40mm. QW403.6

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Prakash.Verma@akersolutions.com
Sent: Friday, January 21, 2011 4:08 PM
To: materials-welding@googlegroups.com
Subject: [MW:9374] Minimum thickness Qualification

 

  

Dear All,

 

If welding base material thickness is 20 mm & impact testing done for this thickness then what is the minimum thickness qualification range ?(As per ASME SEC IX,B 31.3,Asme SEC VIII)

 

Please help friends.

  

--

With Warm Regards,
Prakash Verma
DQC-Drilling Riser Systems
QS Supply Chain.
Aker Solutions Supply chain hub-India
AkerSolutions
Tel.+91-20-66 28 8538
Email. prakash.verma@akersolutions.com

 

 


No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...