Very few manufacturers are requiting the AWS /CSWIP Inspector otherwise required for GULF and other nations.   

 

Regards

M.G.Kattimani

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of syed moinul hasan
Sent: Sunday, January 23, 2011 11:08 AM
To: materials-welding@googlegroups.com
Subject: [MW:9407] cswip/aws

 

dear experts,

do we have any scope of doing AWS/cswip in India? or its only in oil rich gulf nations?

 

regards

Moin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

NOTICE - This communication may contain confidential and privileged information that is for the sole use of the intended recipient. Any viewing, copying or distribution of, or reliance on this message by unintended recipients is strictly prohibited. If you have received this message in error, please notify us immediately by replying to the message and deleting it from your computer.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...