[MW:9452] Operating manual for Fischer Deltascope MP3

I have an old Fischer ferrite meter which has not seen use in several
years. A customer is asking to detemine ferrite content for
production welds. I intend to send the instrument out for calibration
and to perform maintenance as necessary. However, the instrument
manual has some how been lost. Would any have a similar instrument
and be willing to share a coupy of the operating manual. The ID tag
on the back of the instrument reads as follows:

Fischer Technology, Inc.
Deltascope MP3
No. 111-12114A
Made in USA Bat 9V IEC: 6LF22

Front of instrument simply idntifies the meter as: Feritscope

Any help would be greatly appreciated.

Thanks - John

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...