[MW:9453] RE: 9437] Difference between ASNT CP-189 & SNT-TC-1A Reg.,

Dear Mr.KCR

 

ASNT CP-189: ASNT Standard for Qualification and Certification of Nondestructive Testing Personnel 

 

SNT-TC-1A: Personnel Qualification and Certification in Nondestructive Testing

 

SNT-TC-1A, which, with the addition of Codes of Practice ANSI/ASNT CP-189 and ANSI/ASNT CP-105, covers all aspects of qualification and certification of NDT personnel. SNT-TC-1A specifies an employer based certification scheme for Level I and Level II NDT personnel

 

M.Poopandi

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kcrtechnical
Sent: Tuesday, January 25, 2011 8:28 AM
To: materials-welding@googlegroups.com
Subject: [MW:9437] Difference between ASNT CP-189 & SNT-TC-1A Reg.,

 

Dear Friends,

 

Can any nody share with me about  

1) what is      ASNT CP-189   

2) what is      SNT-TC-1A

3)Difference between both

Best regards

KCR

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 9.0.872 / Virus Database: 271.1.1/3400 - Release Date: 01/24/11 10:35:00

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...