Dear team members,
The material spec is super duplex UNS 32760.
Construction code is ASME B31.3.
Operating pressure is 16Bar.
We have bought the elbows and pipe material with the logitudinal weld seam.
During the fabrication we have faced with the problem on elbow to elbow and pipe to elbow welding. The problem is the manufacture weld seams are in the same line as indicated in the attached photos. Is it acceptable?
Please share your experiences.
best regards,
Elshan.
Subscribe to:
Post Comments (Atom)
Re: [MW:34832] Inquiry about Single Bevel with Back Grinding
Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment