hI

HOW TO WELD IS IT A BRANCH OR IF IT IS BRANCH GO FOR SET IN TYPE AND
WELD BY GTAW THEN DO HYD TEST


On Sat, 15 Jan 2011 23:04:54 +0530 wrote
>Dear All,

Is it possible to weld pipe 3/4" to pipe 4" in LP steam service  in the
form of Pipe to Pipe (we have no any sockolet or Halfcoupling, ...)?

Does it need REINFOCEMENT?

your reply is highly appreciable.

 
RegardsZarei




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...