Dear  Sir,

 

Please tell the name of electrode to be used.

 

Thanks and regards.

 

VKJ

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muni Andy
Sent: Monday, January 03, 2011 5:59 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9049] Repair of Body cracks for A 217 Gr WC6

 

Dear Vinod,
It can be welded.But you have to dismantle the valve.
Do preheat as per A217,Weld it and then do Post weld heatreatment
at 700 Deg C.Soaking hours as per thickness.
Do the remachining where required because there
may be little distortion.
Do the crack removal by grinding.
Before proceeding grinding,arrest the crack at both ends.
Regards,
C.Muniyandi
Coimbatore
9994765591

On Sun, Jan 2, 2011 at 9:57 AM, Vinod Jotwani <poojvin@yahoo.com> wrote:

Dear All,

We have noticed multiple crack during the replica check in the control valve body ( Material A 217 Gr WC6 , size 2 " X 2500 RTJ, H2 service) during the fire incident at our Hydrocracker plant.  We would like to carry out the repair jobs for the same,

Kindly share your experience and also advise whether advisable or not. Also share the WPS and cautions to be followed if repair performed by anyone in the group.

Vinod





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Disclaimer: The information in this e-mail and in any files transmitted with it, is intended only for the addressee and may contain confidential and/or privileged material.
Access to this e-mail by anyone else is unauthorized. If you receive this e-mail in error, please contact the sender immediately and delete the material from your computer.
If you are not the intended recipient, any disclosure, copying, distribution or any action taken or omitted to be taken in reliance on it, is strictly prohibited.
Statements and opinions expressed in this e-mail are those of the sender and do not necessarily reflect those of MARAFIQ.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...