Dear All

Most comercial Steels are clasified into 3 categories:-
(a)- Plain Carbon Steels
(b)- Low-alloy Steels
(c)- High-alloy Steels

(a) Plain Carbon Steel is further classified into 4 gorups:-
(1)-Low Carbon Steels often called Mid steels, C-0.3% (more ductile)
(2)- Medium Carbon Steels C- 0.3-0.45% 
(3)- High Carbon Steels C- 0.45-.75% (challenging to weld, Preheat & PWHT)
(4)- Very High Carbon Steels C- upto 1.5% (used for cutting tools, Heating before, during and after welding)

(b)- Low alloy Steels:- Typically below 0.25%c often below 0.15%, typical alloys include Ni, Cr, Mo, Mn & Si which add strength at room temp. and increase low temp. notch toughness which would include C-Mn steel, Quenched and Tempered Steel and HSLA steel.

(C)- High alloy Steels:- Very little amount of C upto .30%, other alloys would include Cr, Mo, Ni etc. for Eg:- Stainless Steel & Cryogenic Steels.

Now i would like you to explain your query in detail....

Regards
Manpreet Singh 




On Wed, 05 Jan 2011 11:42:19 +0530 Sundaram Sundaram wrote
>
Hi Friend,
                  Regarding the alloy steel.If the steel contains upto 5% of alloying element then it is called as low alloy steel.If more than 5 - 10 % medium alloy steel,more than 10% high alloy steel.
 
with thanks,
N.Shanmuga sundaram
>
>
On Wed, Jan 5, 2011 at 9:55 AM, Sundaram Sundaram <nss2410@gmail.com> wrote:
>
Hi Friend,
                  Dont confuse with all these explanation.The simple way,the basic metallurgy says the material which contains upto 2% carbon is accounted as steel.Above 2% carbon it is considered as cast Iron.You can confirm with IRON-CARBON equilibrium diagram
 
with thanks & regards,
N.Shanmuga sundaram,
QA/QC Welding/painting Inspector,
Moody International,
UAE
>
On Wed, Jan 5, 2011 at 8:25 AM, Barry Gideon <barry@arv-offshore.com> wrote:
>

Can anyone advise me where I can find the definition for CARBON STEEL and LOW ALLOY CARBON STEEL (Preferably an explicit definition by ASTM and the relevant standard number/description).

 

Form a web search I have found the following definitions :

AISI defines carbon steel as follows: Steel is considered to be carbon steel when no minimum content is specified or required for chromium, cobalt, columbium [niobium], molybdenum, nickel, titanium, tungsten, vanadium or zirconium, or any other element to be added to obtain a desired alloying effect; when the specified minimum for copper does not exceed 0.40 per cent; or when the maximum content specified for any of the following elements does not exceed the percentages noted: manganese 1.65, silicon 0.60, copper 0.60.

Alloy or alloyed steels are defined by the ISO specification 4948/1 in the following manner. Alloy steels are those containing any element listed below in a quantity equal to or greater than the quantity for that listed element: aluminium 0.10%, boron 0.008%, bismuth 0.10%, chromium 0.30%, cobalt 0.10%, cupper 0.40%, manganese 1.65%, molybdenum 0.06%, lead 0.40%, selenium 0.10%, silicon 0.50%, tellurium 0.10%, titanium 0.05%, tungsten 0.10%, vanadium 0.10%, zirconium 0.05%, Lanthanides (each) 0.05%, other specified elements (except carbon, sulphur, phosphorus, nitrogen) 0.05% [Ref 1].

Various attempts have been made to distinguish 'low' and 'high' alloy carbon steels, but the definitions vary between countries and between standard-setting organisations. As a general indication, low alloy steel can be regarded as alloy steels (by the ISO definition) containing between 1% and less than 5% of elements deliberately added for the purpose of modifying properties.

However, AISI defines low alloy steels as a constitute to a category of ferrous materials that exhibit mechanical properties superior to plain carbon steels as the result of additions of alloying elements such as nickel, chromium, and molybdenum. Total alloy content can range from 2.07% up to levels just below that of stainless steels, which contain a minimum of 10% chromium.

 

Regards

 

 

Barry Gideon

           

ARV Group Logo small (Arpprove 25-10-2007)

ARV Offshore Co., Ltd.

555 Rasa Tower 2, 18th Floor

Phaholyothin Road, Jatujak, Bangkok 10900

THAILAND

Tel:       + 66 (0) 2937 1211
>
Fax:      + 66 (0) 2937 1212
>
Mobile: + 66 (0) 8 4705 0588

Skype:     Barry_Gideon

P Save a tree...please don't print this e-mail unless you really need to

 

"The information contained in or attached to this e-mail is confidential and may be subject to legal or professional privilege.  This e-mail is intended to be reviewed only by the individual to whom it is addressed, as named above.  If you are not the intended recipient or an authorized representative of the intended recipient, you are hereby notified that any review, dissemination or copying of this e-mail and its attachments, if any, or the information contained herein is prohibited.  If you have received this e-mail in error, please immediately notify the sender by return e-mail and delete this e-mail and any attachments permanently from your system.  Thank you."

 


>
Any business communication, sent by or on behalf of ARV Offshore Co Ltd, ARV Holdings Pte Ltd or one of its affiliated firms or other entities (together "ARV"), is confidential and may be privileged or otherwise protected. If you receive it in error please inform us and then delete it from your system. You should not copy it or disclose its contents to anyone. Messages sent to and from ARV may be monitored to ensure compliance with internal policies and to protect our business. Emails are not secure and cannot be guaranteed to be error free. Anyone who communicates with us by email is taken to accept these risks.
>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

>

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...