RE: [MW:9109] Regarding batch qualification for EC308L

Dear Prem

 

Thanks for the reply.

 

Actually I have gone through SFA 5.9,Please look at clause no 7 .& clause no A 10.3.

 

Now Question arises that, as per SF1 5.9,Only chemical test is required. If any how we want to check impact test, fillet test & radiographic test, then which SFA should we follow? As per clause A10.3 Is it SFA5.4? If yes then for 1.2 mm dia  wire what steps we should take for further all these  testings.

 

All members Please suggest on this matter.

 

Thanks & regards

Vinit

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREM SHANKARDUTT NAUTIYAL
Sent: Wednesday, January 05, 2011 4:06 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9101] Regarding batch qualification for EC308L

 


Dear Vinit

The MIG wire you are referring is a composite cored wire.

Please refer ASME Sec II Part C, SFA 5.9 wherein you will get all the tests to be conducted for batch qualification.

Regards

Prem Nautiyal


On Wed, 05 Jan 2011 14:33:47 +0530 wrote
>Dear all,

we want to take batch test qualification for EC 308LMIG welding(1.2MM DIA) .Can we know which tests will be applicable for this? also please send all lthe details( such as thickness of base metal ).We also want to carry out impact @-196C for this .Please share information regarding this.

Regards
Vinit




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9769316004

Image removed by sender.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...