Re: [MW:9111] grinding or cleaning of stainless steel



Dear all,

galvanic corrosion in austenite stainless steel?


Regards,
Pankaj

On Tue, Jan 4, 2011 at 6:49 PM, Ali Asghari <asghariali@rocketmail.com> wrote:
Dear All
what is suitable material for rasp or chisel for austenite stainless steel due to prevention of galvanic corrosion?
is there a risk if used from ordinary material?
regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...